Skip to content
MotorsCNC
Get a quote

Home / Processes

How Motor Housings and Shafts Are Machined

A motor part is judged on a few features: two bearing seats on one axis, a stator bore that stays round, journals that run true. This page goes through the processes that produce those features, in the order a shop runs them, so you can tell what your drawing is asking for and check that a quote covers it.

Written by the team that reads your RFQLast reviewed How we write these

Which process makes which feature

Typical pairings and typical results on a stable part. The shop that quotes you confirms what it can hold on your geometry and your blank.

FeatureUsual processTypical result
Bearing seats in a housing or end bellFinish boring, same setup as the stator bore where possibleH7 typical, H6 on precision seats. Ra 0.8 to 1.6 µm
Stator bore (shrink or press fit)Rough and finish boring, roundness checked after unclampingInterference set by the designer. Roundness often 0.01 to 0.03 mm
Shaft bearing journalsTurn soft, heat treat, then cylindrical grind (or hard turn)±0.005 mm after grinding, IT5 to IT6 class. Ra 0.2 to 0.4 µm
Rotor stack seat on the shaftTurning, sometimes knurled or ground for a press fitSet by the stack press-in force the designer wants
KeywaysEnd milling, or broaching in a hub boreWidth per the key standard on the drawing (DIN 6885, ANSI B17.1)
SplinesHobbing, shaping, rolling or broachingPer the spline standard on the drawing (ISO 4156, DIN 5480, ANSI B92.1)
Flange spigots and mounting facesTurning or milling in the bearing seat setupRunout to the bearing axis, often 0.02 to 0.05 mm
Water jacket and sealing facesMilling, then leak testFlatness 0.03 to 0.05 mm on a gasket face is common

H7 is definitional under ISO 286: the lower limit is the nominal size and the band is IT7, so a 62 mm H7 seat runs from 62.000 to 62.030 mm. Shaft classes such as k5, k6 and m6 are named but not tabulated here, because public sources disagree on the deviations. Use your bearing maker's table. Bore limits by size are on the bearing seat fit reference.

Turning rotor shafts

Rotor and armature shafts are usually 1045 or 4140 steel, stainless 303 to 316 for wet duty. The sequence below is the common one for a shaft with ground journals.

  1. Turn between centres

    Centre drill both ends first. Every later operation, grinding and balancing included, locates on those centres, so they set the runout of the finished shaft. Long shafts get a steady rest.

  2. Cut keyways and splines soft

    Keyways, splines, threads and cross holes are cut before hardening while the steel still machines easily. Splines on production shafts are usually hobbed or rolled.

  3. Heat treat

    4140 bar is often bought quenched and tempered and machined as is. Journals that need wear resistance are induction hardened locally, which leaves the core tough and the splines soft unless they are hardened too.

  4. Grind or hard turn the journals

    Cylindrical grinding between the same centres takes journals to final size and finish. Hard turning with CBN inserts can replace grinding on some journals, which saves a machine and a queue.

Hollow shafts for cooling or cabling start from seamless tube or are gun drilled from bar. Either way the bore has to run true to the journals, which is easier to hold when the outside is finished after the bore.

Boring housings and bearing seats

The housing carries the stator and, through its end bells, both bearings. What matters is that the stator bore and the two bearing seats share one axis. The more of those features a shop cuts in a single clamping, the less alignment error builds up.

On a round housing that usually means a turn-mill or a lathe with live tooling: stator bore and the near bearing seat in one setup, then the part flipped onto a fixture that locates in the finished bore for the far end. On larger or non-round frames a horizontal machining center bores from both sides on a rotary table, or line bores through both seats with one long bar.

Finish boring

A seat at H7 or tighter gets a separate finish boring pass with a fine-adjustable boring head, after the roughing heat has left the part. The operator gauges it with a bore gauge or air gauge, not calipers. H8 seats can often be finished with an interpolated end mill. This difference is one of the biggest single price drivers on a housing.

Thin walls and roundness

Aluminium housings with thin walls deflect under jaw pressure. A bore that is round while clamped springs out of round when released. Shops counter it with low clamping force, more contact area, a rough cut followed by unclamping, and a light finish cut. The stator bore is checked for roundness after release, not on the machine.

Stator shrink fits

Many stators go into the housing on an interference fit: the housing is heated so the bore opens, the stack drops in and is gripped as it cools. The bore diameter, its roundness and the finish decide how evenly the stack is held. Aluminium grows about twice as much as the steel stack with temperature, so the designer sets the interference to keep grip at the hottest running point.

Grinding

Cylindrical grinding between centres finishes journals, seal diameters and shoulders that a bearing locates against. Plunge grinding does a journal and its shoulder in one pass. Centreless grinding suits pins and simple shafts without features that block the wheel. Ground journals typically reach ±0.005 mm and Ra 0.2 to 0.4 µm. Grinding burn, from a dull wheel or too much infeed, softens hardened journals and is checked by etch or Barkhausen noise on critical shafts.

Balancing

Balance grades come from ISO 1940-1, now published as ISO 21940-11. Electrical armatures typically sit at G6.3, or G2.5 with special requirements. Balancing happens at assembly, so the drawing should say where correction is allowed: a rim that can be drilled, a ring that can be turned, or balance weights. The permissible unbalance for your rotor mass and speed is on the balance grade calculator.

Lamination stacks: what the machine shop does and does not touch

Stator and rotor cores are stacks of thin electrical steel sheet, insulated from each other to limit eddy currents. Common grades are written to IEC 60404-8-4 and EN 10106 (for example M270-35A or M330-50A, loss and thickness in the name), JIS C 2552 in Japan, or ASTM A677 in North America. The sheets are stamped or laser cut, then held together by interlocking tabs, welding along the outside or bonding.

The machine shop mostly works around the stack, not on it. Its jobs are the housing bore the stator sits in, the shaft seat the rotor stack is pressed onto, and sometimes the end rings. Machining across a finished stack is avoided because the cutter drags burrs across the sheet edges and can short laminations together. When a light skim of a rotor outside diameter is unavoidable, sharp tools and light cuts limit the damage, and the drawing should say it is allowed.

Before the stack is pressed on, the shaft seat may be knurled or ground to control press-in force. Say on the RFQ whether the shop supplies the bare shaft or the shaft with stack fitted, because the second is a different job.

Machining die-cast housings

At production volume most aluminium housings start as high pressure die castings, often ADC12 or A380. Materials compared on the motor part materials reference. Four things decide whether the machined part is good.

Cast datums

The first operation locates on datum targets on the raw casting, the points the caster and the machinist agree on. If the drawing does not show them, the shop picks its own and the cast walls may end up off center to the bores.

Stock allowance

High pressure die castings typically carry 0.5 to 1.5 mm of machining stock on finished faces. Too much and the cutter reaches porous metal below the dense skin. Too little and the bore does not clean up.

Porosity

Gas and shrink porosity open up when a face is machined. Sealing faces and water jackets are leak tested, and porous castings may be vacuum impregnated after machining. Say on the RFQ which faces must be free of visible pores.

Tooling at volume

ADC12 and A380 are abrasive because of their silicon content. Production lines run PCD tools on aluminium housings for tool life and consistent bore finish.

Drawing notes that make the process cheaper

  • Tolerance the bearing seats and journals tightly, and open everything that does not locate a bearing or the stator.
  • Call coaxiality or runout between the two bearing seats against one datum axis.
  • Name the bearing and fit class, not only a diameter with limits.
  • Show datum targets on a casting drawing, and which faces must be free of visible porosity.
  • Give shaft speed with the balance grade, and show where correction material may be removed.
  • State the leak test method and pressure for any water jacket.

What we do

We read your RFQ, quote the finished parts and place the work with a partner shop that runs the processes your drawing calls for. We reply within 24 business hours. How we choose a shop is on the partner shop page.

Questions about the processes

Do I need ground journals, or is a turned shaft enough?

It depends on the bearing fit and the finish. A turned journal on a soft shaft can hold a loose bearing fit. A diameter tolerance under about 0.01 mm, a finish under Ra 0.4 µm or a hardened journal usually needs a grinder, or a shop that hard turns. Name the bearing and the fit class on the drawing so the shop can tell which.

Why should the stator bore and bearing seats be machined in one setup?

Because the air gap depends on the rotor running concentric to the stator. Every time a part is unclamped and reclamped, alignment error is added. Boring the stator bore and at least one bearing seat in the same setup, then locating the end bell seat off that axis, is the usual way to hold coaxiality.

Does the machine shop balance the rotor?

Usually not. The rotor is balanced at assembly once the lamination stack, fan and anything else on the shaft is fitted. The shop controls the geometry that makes balancing work: concentric journals, true centres and material left where correction holes or cuts go.

Can a lamination stack be machined?

It can, but it is avoided where possible. Cutting across a stack smears burrs between the sheets and can short them together, which raises eddy current loss. Stacks are normally stamped or laser cut to size and only skimmed lightly when a drawing calls for it.

Standards and references

  1. ISO 286-1, Geometrical product specifications, ISO code system for tolerances on linear sizes. IT grades and the H hole basis used for bearing seats.
  2. ISO 21940-11, Mechanical vibration, Rotor balancing, Part 11: Rigid rotors (formerly ISO 1940-1). Balance quality grades.
  3. Electrical steel, Wikipedia. Why laminations are insulated and why shorted sheets raise loss.
  4. IEC 60404-8-4, Magnetic materials, Specifications for cold-rolled non-oriented electrical steel strip and sheet. Grade naming such as M270-35A.

Figures on this page are typical ranges drawn from the standards above and from ordinary shop practice. They are not a specification for your part. The partner shop that prices your part confirms what it can hold on your geometry.

Get a quote for your motor part