Materials for Motor Housings and Shafts
Four materials cover most of the motor parts that come through an RFQ. Here is how they compare, side by side.
Written by the team that reads your RFQLast reviewed How we write these
| Material | Form | Typical tensile strength | Elongation | Machinability | Typical use |
|---|---|---|---|---|---|
| 6061-T6 | Wrought bar / plate | ≈ 310 MPa (45 ksi) | Moderate to high | Good | Prototype and low volume housings, end bells |
| A356-T6 | Sand or permanent mould casting | Low 200s MPa, process dependent | Low to moderate | Good | Mid to high volume housings |
| ADC12 | Die casting | Similar range to A356, lower ductility | Low, under a few percent | Fair, watch surface porosity | High volume housings |
| 4140 | Bar, various heat treat conditions | Wide range, set by heat treat | Set by heat treat | Depends on condition | Rotor and drive shafts |
Ranges are typical figures for the alloy and process combination, drawn from the sources below. They move with casting process, section size and heat treat condition, and are not a substitute for your supplier's own datasheet.
Why the machine shop rarely picks between them
By the time a drawing reaches a shop, the material is almost always fixed. A motor's thermal and structural design assumes a specific alloy, particularly for the housing, where wall thickness and heat rejection are already calculated against it. Asking a shop to substitute one for another is a design question, not a machining one.
What does change the quote is the exact condition: 6061-T6 versus 6061-T651, 4140 annealed versus quenched and tempered. That detail is worth checking before the RFQ goes out, because it changes machinability, cycle time and, on a shaft, whether the part can hold the tolerance you asked for.
The reasoning behind each of the four materials, and why each gets picked, is in the full materials guide.
Questions about the table
Why are these given as ranges instead of single numbers?
Because a single number would be false precision. Cast alloy properties depend on the casting process (sand, permanent mould or die), and steel properties depend entirely on heat treat condition. The alloy standard defines chemistry, not a guaranteed mechanical property. A datasheet from your actual caster or bar supplier, for your actual process, is the number to design against.
Which of these can a machine shop substitute on its own?
None of them, and a shop that machines motor parts for a living will not offer to. Material choice is normally set by the motor designer, not by whoever is cutting the metal. The one thing worth confirming on an RFQ is the exact temper or heat treat condition, since it is sometimes left off a drawing.
Is there a fifth material that should be on this table?
A380/383 die casting alloys are the North American near-equivalent to ADC12 and show up on drawings from US-specified suppliers. We kept this table to the four alloys that appear most often on the RFQs we see. Tell us at the address below if another one belongs here.
Standards and references
- Aluminum Association, International Alloy Designations and Chemical Composition Limits for Wrought Aluminum and Wrought Aluminum Alloys. Composition and temper designations for 6061.
- ASM Handbook, Volume 2: Properties and Selection of Nonferrous Alloys and Special-Purpose Materials. Typical mechanical property ranges for 6061-T6 and A356-T6.
- JIS H5302, Aluminium alloy die castings. The Japanese Industrial Standard defining ADC12.
- SAE J404, Chemical Compositions of SAE Alloy Steels. Defines the 41xx series 4140 belongs to. Mechanical properties depend on heat treatment, not this standard.
Figures on this page are typical ranges drawn from the standards above and from ordinary shop practice. They are not a specification for your part. The partner shop that prices your part confirms what it can hold on your geometry.